Polished Concrete Kitchen Floors: A London Guide to High-End Kitchens and Extensions

Most of the polished concrete floors we pour in London homes are kitchens, and most of those are in extensions: a rear or side return, a lower ground opened up, a town house pushed out under a glazed roof. It is the room where the material makes most sense, and the room where the decisions matter most.
This guide is for homeowners planning one, and for the architects and builders working with them. It covers how the floor is made, what it looks like to live with, underfloor heating, what your builder needs to know, and when we would talk you out of it.
The short answer
A polished concrete kitchen floor is usually a new 100 mm slab, coloured and power-floated on pour day, cured for three weeks, then burnished and sealed. It suits extensions and ground-floor refurbs where the floor is coming up anyway, works well over underfloor heating, and runs seamlessly from the kitchen to the glass. Allow four to five weeks from pour to finished floor, and expect a surface that is mottled, not uniform. We install floors from around 30 m² upwards.

Why the extension is where it belongs
The floor is being built from scratch anyway, so making the slab the finished floor removes a whole layer, with its grout lines, movement and height build-up. The rooms are big, open and bright, and they want one uninterrupted plane. In St John’s Wood, 320 m² of polished concrete in two tones, white on the lower ground and a deeper grey below, turned a basement extension into the brightest part of the house, because a pale concrete floor bounces daylight rather than absorbing it.
How the floor is made
We lay a reinforced 100 mm slab, broadcast a dry colour hardener into the surface while the concrete is wet and power-float it in. The colour and the soft sheen come from the hardener and the float, not from grinding. The next morning we cut the control joints. The slab then cures for at least 21 days under protection while the build carries on around it. We return to fill the joints with a colour-matched filler, shave them flush, burnish the surface to the agreed sheen and seal it. Two visits, four to five weeks end to end.
Want more texture? The same slab can be ground back after curing to expose the stone in the mix, then polished: a terrazzo-like floor with real depth, as under the oak frame of the Pump House barn in Pinner.

What it looks like, and what it doesn’t
A colour-hardened floor is a natural, trowelled surface. Trowel passes, density shadows and slightly different edges are the finish, not defects, and no two floors come out the same. If you want one flat, even colour like a resin, concrete is the wrong choice and we will say so.

Colour is a direction, not a match. We choose from a chart and a sample, and the floor sits in the range of that colour. Look at the sample in your room, in your light, at the time of day you use the kitchen most. A north-facing London room cools a tone down; a glazed roof warms it up. Our finish selector shows the nine finishes on floors we have installed.
Joints will show. Every slab needs control joints so it cracks where we intend and nowhere else: a line at the threshold to the old house, and a grid of roughly six metres on larger floors. Filled and shaved flush, they read as quiet lines in the floor, and if your architect places them with the island and the glazing bars in mind, they become part of the design.
Pairings that work: pale concrete with oak and brass; mid grey against dark joinery and a stone worktop; a warm sandy tone under a white kitchen that would otherwise feel clinical. The floor is the largest surface in the room. Decide it first and let the joinery answer it.
Underfloor heating
Polished concrete and underfloor heating are a natural pair: a dense slab with no covering holds heat and releases it slowly. Most kitchen floors we pour have pipes in them. The rules are strict, because heat on young concrete is the surest way to ruin a floor. The pipes are pressure-tested and kept under pressure through the pour and cure. The heating stays off until seven days after sealing, then comes up gradually over several days, and is raised and lowered gently at the start and end of every heating season for the life of the floor.
What your builder needs to know
Before we pour: groundworks, insulation, damp-proofing and heating pipes complete; the finished floor level agreed in writing; the engineer’s reinforcement and joint positions received; the colour signed off; the building weathertight and enclosed. Wind, draughts and direct sun on pour day spoil the surface in its first few hours, so an extension without its glazing in is not ready.
During the cure: the site works over protection. We issue the cure rules to your builder in writing before we leave, and check them before we return; the boards come off five to seven days ahead so the slab can breathe. Ideally the slab goes in before stud walls, plasterboard and skirtings, so the floor runs clean to the structure. Agree this before the programme is fixed, not after.
The programme at a glance
| Stage | How long | What happens |
|---|---|---|
| Visit 1 | 2–3 days | Mesh and preparation; pour, colour hardener and power float; joints cut and the slab covered the next morning |
| The cure | 21 days minimum | Your build carries on over protection. Heating off. Boards lifted 5–7 days before we return |
| Visit 2 | 2–3 days | Clean, fill the joints flush, burnish to the agreed sheen, seal |
| After sealing | 7 days, then 4 weeks | No foot traffic for 24 hours; soft shoes and dry cleaning for a week; heating on gradually from day 7; rugs from week 4 |
Typical programme for guidance; we confirm every date in writing before other trades programme against it.
Living with it
Dust-mop to keep grit off, damp-mop with a pH-neutral cleaner, buff dry. No vinegar, lemon, descalers, bleach, steam mops, waxes or rubber-backed mats. The sealer buys time with a spill; it does not make the floor stain-proof, so wine and oil are blotted, not left. Repairs will show. In a busy walkway the sheen softens over the years, and a maintenance clean and re-seal brings it back.
When we’d talk you out of it
- You want a uniform, even colour. Choose a resin or a large-format tile.
- You need the floor in one visit, or the programme cannot hold a three-week cure.
- The kitchen is on an upper floor or a timber structure without an engineer’s design for a 100 mm slab.
- The floor is under around 30 m².
Extension already built? If the floor underneath is sound, there is another route: LPC Hardcrete microcement, about 3 mm thick, applied over the existing floor in a week, seamless, and able to run up the island and the walls. We did exactly that at Barrowgate Road in Chiswick. Here is how the two compare.

What it costs
It depends on the finish, the area and what the site needs from us, so rather than one figure here, see the polished concrete price guide for London: the per-square-metre range by finish and what moves it.
Two questions we always get
Is it cold underfoot? It takes the temperature of the room or the pipes within it. With underfloor heating it is one of the warmest floors you can stand on; without, it feels like stone.
Does it crack? Concrete moves, which is why we cut the joints. Cracks outside the joints come from joints cut late, a poor sub-base or heating switched on too early, all of which the programme above prevents.
Planning a kitchen extension?
Send us the drawings. We will tell you which finish suits the room, where the joints should fall and what the programme needs from your builder, before the start date is fixed.